Welding electrode for patinated steel type Corten - E8018-W2

Code: 8018250KS 8018250 8018250KR Choose variant
BLACK FRIDAY
€0,40 / pcs €15,88 / kg €63,50 / package from €0,40 / pcs €0,48 incl. VAT €19,21 incl. VAT €76,84 incl. VAT from €0,48 incl. VAT
Skladem (>100 pcs) Skladem (10.2 kg) Skladem (2 package) Choose variant
Průměr
Balení
Chosen variant is not available. Reset selected parameters.
Delivery to:
09/12/2025 09/12/2025 09/12/2025 Choose variant
Delivery options

Detailed information

Product detailed description

Electrode E8018-W2 for welding of patinated Corten steels

Basic electrode for welding of COR-TEN patinated steels with very low hydrogen and carbon content. The electrode cover, containing an extruded moisture resistant alkaline flux, helps to ensure a controlled electrode penetration. Electrode yield 120 %. Smooth arc, low spatter, easy ignition and re-ignition. Specifications: AWS E8018-W2.

The electrode is mainly used for welding weathering resistant steel. The weld metal is resistant to corrosion in seawater, especially in Arctic waters with high oxygen and salinity. It is suitable for welding micro-alloyed carbon-manganese steels in icebreakers and offshore structures, for architectural structures, bridges, etc.

For welding steels: Corten A, B1 (US Steels), PATINAX, DILLICOR, BS4360 Grade WR50A to WR50C, ASTM A588 Grade A, B, C, K. DIN 1.8960, 1.8961, 1.8963.

corten_design_small corten-steel-bridge_small corten_facade_small

Typical weld metal composition (%)

C

Si

Mn

P

S

Cr

Ni

Mo

Cu

0,06

0,60

1,00

0,015

0,010

0,60

0,60

0,02

0,50

Mechanical properties of weld metal

Minimum

Typical

Rm/Tensile Strength

N/mm2

550

610

Rp0.2% Proof Stress

N/mm2

460

520

A5 / Elongation

4d (%)

5d (%)

25

20

Area reduction

%

65

Impact Energy -20°C

J

150

Impact Energy -40°C

J

100

Impact Energy -60°C

J

70

Impact Energy -20°C

J

40

Welding parameters. DC+ / AC min 70 V)

Electrode diameter

Welding current

2.50 mm

70-100 A

3.25 mm

80-140 A

4,00 mm

100-180 A

5.00 mm

140-240 A

To ensure a low hydrogen content in the weld metal < 5 ml/100, only dry electrodes must be used. If the electrodes become wet, they must be dried at 300-350°C for 1-2 hours. Do not exceed 420°C!

Additional parameters

Category: LOW ALLOY STEELS
běžná ocel: běžná ocel
Mn ocele: manganové ocele
obal: bazické

Be the first who will post an article to this item!