Electrode for repair of cast iron castings CHEM-WELD 6200

Code: 6200250KS 6200250 6200250KR 6200325KS 6200325 6200325KR Choose variant
BLACK FRIDAY
€2,91 / pcs €103,82 / kg €519,10 / krabička €3,43 / pcs €103,82 / kg €519,10 / krabička from €2,91 / pcs €3,52 incl. VAT €125,62 incl. VAT €628,11 incl. VAT €4,14 incl. VAT €125,62 incl. VAT €628,11 incl. VAT from €3,52 incl. VAT
14-30 dní / na objednávku 14-30 dní / na objednávku (0.022 kg) 14-30 dní / na objednávku Skladem (>100 pcs) Skladem (15.94 kg) Skladem (3 krabička) Choose variant
Průměr
Balení
Chosen variant is not available. Reset selected parameters.
Delivery to:
- - - 09/12/2025 09/12/2025 09/12/2025 Choose variant
Delivery options

Electrode for welding and repair of cold cast iron castings

Detailed information

Product detailed description

CHEM-WELD 6200

Electrode for cold welding of new cast iron

Electrode suitable for welding and repairing new cast iron and for welding cast iron to steel, for grey and tempered cast iron, for steel to steel and copper and copper alloyed cast iron.

  • for the removal of defects after casting
  • for welding out badly drilled holes

The welds can be further processed, e.g. by grinding.

The colour of the weld metal is identical to the base material.

When welding grey cast iron, 3 basic rules must be observed:
 
Welding should only be carried out in short caterpillars
1 to 3 cm - the length of the caterpillar should approximately correspond to the thickness of the part to be welded.
2. Immediately after welding, hammer (tool) with a round (blunt) nose 
- never with a sharp tool
3. Interpass temperature 
- place the next caterpillar when you
keep your bare hand on the weld

ADVANTAGES

welding without preheating

also suitable for transformer

transition

DISADVANTAGES

does not have

When welding cast iron, it is necessary to follow the technological procedure.

SPECIFICATIONS

CHEM-WELD 6200

Electrode for cold welding of new cast iron

DIN 8573: E Ni Fe-1-BG13

AWS A 5.15: E Ni Fe-Cl

EN ISO 1071: ECNiFe-Cl3

Packaging: rutile-basic

Welding current:~40V/=+

Welding position: PA, PB, PC, PD, PE, PF, PG

Electrode for repairs on new cast iron, for welds to be further worked, for welding ductile iron with steel, for grey cast iron, for steel lithium. Fine grinding of transitions on solid cast iron parts is possible. The colour of the weld metal is identical to the base material.Particularly tough and crack resistant. For welding and repairs, for removing casting defects on engine blocks, repairing broken cast iron parts, welding out badly drilled holes, machine housings. Necessary short welds and hammer peening, welding at low currents.

Typical chemical composition of weld metal [%]:

C

Si

Mn

Ni

Fe

1,0

<2,0

<1

56

residue

Mechanical properties of weld metal:

Rm [MPa]

Re [MPa]

A5 [%]

Hardness [HB]

>400

350

20

200

Drying: Generally no drying required

Diameter [mm]

Length [mm]

Number [pcs in kg]

Packing /kg

Welding. Current [A]

2,50

350

49

5,0

50-80

3,25

350

30

5,0

70-110

4,00

350

21

5,0

90-130

Additional parameters

Category: CAST IRON
běžná ocel: běžná ocel
litina: litina
ocelolitina: ocelolitina
měď: Měď
různé ocele: různé ocele k sobě
trafo: na trafo
Balení: ks, kg, krabička
Průměr: 2,50 - 3,25 mm
5
3x
4
0x
3
0x
2
0x
1
0x
Do not fill out this field:

List of ratings

5
KF Avatar of author | 24/07/2025
Velice . dekuji

Společnost CHEM-WELD byla založena v  Rakousku roku 1967 panem Siegfriedem Schweigerem.

Název CHEM-WELD znamená spojení chemie a svařování.

Prvním výrobkem bylo speciální lepidlo na kov Chem-Stahl 1000 HT,  které nahrazovalo svařování v dolech JAR.

vystava_bvv_1994_chemweld